产品 · 参数
标准 | 化学成分(W%) | 对应国际标准 | ||||||||
C | Si | Mn | Ni | Cr | Mo | Cu | P | S | ||
ISO 21988/JN/ HBW555XCr13 | 1.8-3.6 | ≤1.0 | 0.5-1.5 | ≤2.0 | 11.0-14.0 | ≤3.0 | ≤1.2 | ≤0.08 | ≤0.08 | EN-GJN-HV600(XCr11) ASTM A532 12% Cr |
ISO 21988/JN/ HBW555XCr16 | 1.8-3.6 | ≤1.0 | 0.5-1.5 | ≤2.0 | 14.0-18.0 | ≤3.0 | ≤1.2 | ≤0.08 | ≤0.08 | EN-GJN-HV600(XCr14) ASTM A532 15% Cr-Mo AS 2027 CrMo 15 3 G-X 300 CrMoNi 15 2 1 |
ISO 21988/JN/ HBW555XCr21 | 1.8-3.6 | ≤1.0 | 0.5-1.5 | ≤2.0 | 18.0-23.00 | ≤3.0 | ≤1.2 | ≤0.08 | ≤0.08 | EN-GJN-HV600(XCr18) ASTM A532 20% Cr-Mo AS 2027 CrMo 20 1 G-X 260 CrMoNi 20 2 1 |
ISO 21988/JN/ HBW555XCr27 | 1.8-3.6 | ≤1.0 | 0.5-2.0 | ≤2.0 | 23.0-30.0 | ≤3.0 | ≤1.2 | ≤0.08 | ≤0.08 | EN-GJN-HV600(XCr23) ASTM A532 25% Cr-Mo AS 2027 Cr27 LC & Cr27 HC G-X 260 Cr27 |
ISO 21988/JN/ HBW600XCr35 | 3.0-5.5 | ≤1.0 | 1.0-3.0 | ≤1.0 | 30.0-40.0 | ≤1.5 | ≤1.2 | ≤0.06 | ≤0.06 | AS 2027 Cr35 |
ISO 21988/JN/ HBW600XCr20Mo2Cu | 2.6-2.9 | ≤1.0 | ≤1.0 | ≤1.0 | 18.0-21.0 | 1.4-2.0 | 0.8-1.2 | ≤0.06 | ≤0.06 | AS 2027 CrMoCu 20 2 1 |
性能 · 特点
产品性能
材质:高铬耐磨铸铁;
标准:AS 2027;
硬度:≥HRC60;
尺寸:客户定制
产品特点
采用砂铸工艺制造高铬铸铁提升条。
对高铬铸铁件进行淬火和回火处理以达到理想硬度。